- 8023: Automotive Hydraulic Brake Tube: The Case for 90-10 Copper Nickel Tubing
 
 
The results of extensive corrosion testing and 15 years of use by Volvo show that C70600 copper-nickel tube is superior to the coated steel tube used in today's U.S.-made vehicles. Reprint, SAE Technical Paper, March 1993.- A8001: Copper - Nickel Automotive Vehicle Brake Tubing
 
 
  
 [199 KB] 
Describes growing usage of Copper Alloy No. C70600 (90-10 Cu-Ni) for automotive brake lines. Compares the strength properties and corrosion resistance of 90-10 copper-nickel tube with traditional copper-brazed, double-wrapped, coated steel tube.- 801/2: Procedure for Manufacturing and Testing Tensile-Peel Test Specimens
 
 
Describes specimen preparation and test procedures for evaluating the strength of soldering joints in copper and brass automotive radiator materials.
(4 pgs.) 1 free (add’l $1.00 ea)- 805/08: Process Improvements in Soldering Automotive Radiators
 -  
 [1.6 MB] 
Summarizes CDA's experimental programs on the interrelationships between copper alloy, solder composition, flux formulation and process parameters.